Use of "Black-Box" Reviews in PHA Scenario Development and Validation Against Vessel Limits

King, R.


ABSTRACT:

This presentation will review examples of fitness for service limitations and the potential process safety hazards presented if exceeded.  The use of the “black-box” historical operating data review methodology in PHA scenario development and validation will be discussed.  Fitness for service evaluation of vessels under a time dependent failure mechanisms (hydrogen damage) will also be presented.   

King, R., “Use of "Black-Box" Reviews in PHA Scenario Development and Validation Against Vessel Limits,” Saudi Aramco Global Reliability Forum SAGRF, Houston, Texas, June, 2013